Abstract

In this study, nanocrystalline 3 mol % yttria-stabilized tetragonal zirconia polycrystalline (Y-TZP) ceramic was produced by sintering with a high-frequency induction heating (HFIH) system of granular powders obtained by ultrasonic spray pyrolysis (USP) at 600 °C. The granular nano-sized powders (10-30 nm) were micron in size (average size: 700 nm), spherical in shape and amorphous. The influences of the HFIH sintering temperature (1400-1600 °C), applied current time (60-300 sec.) and the mechanical pressure (10 MPa and 20 MPa) on the final density and grain size of the products were investigated. The amorphous granular Y-TZP powders compressed with the HFIH system allow very rapid condensation in the tetragonal phase at high density and avoid grain growth. High density (relative density over 95) nanocrystalline Y-TZP ceramic with ∼70 nm size could be obtained from the simultaneous application of 20 MPa pressure and an induced current within 300 sec. of sintering time at 1500 °C. In this condition, the sample’s maximum hardness and fracture toughness values were reached at 14.9 GPa and 3.8 MPa·m1/2, respectively. Y-TZP powders produced in nano-micro structure with the USP system were sintered with the HFIH system and rapid production was achieved by preventing grain growth.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call