The properties of quartzite mixtures with various hardening agents with a binder of an aqueous solution of liquid glass with a density of 1.12–1.15 g/cm3 are studied. It is shown that the best hardeners that can replace ferrochrome slag are metallurgical slag and an aqueous formate-alcohol solution (a by-product of production of pentaerythrite).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.