Abstract

An aluminium metal matrix composite reinforced with continuous unidirectional α-alumina fibres has been compression tested at quasi-static and dynamic strain rates. In the transverse direction, the composite showed increasing flow stress (at 5% strain) and maximum stress within the studied strain rates, 10−3−3 × 103 s−1. In the longitudinal direction, the maximum stress of the composite increased similarly with increasing strain rates within the range 10−5−7 × 102 s−1. It is shown that, if brooming of the sample ends can be suppressed, the failure stress of the composite in longitudinal compression increases significantly. Metallographic observations reveal the typical modes of damage initiation in the composite.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.