Abstract
Cast Al-alloy components often exhibit significant variability in fracture-related mechanical properties, such as ductility and strength. In this contribution, the variability in the ductility of tensile test specimens of squeeze cast A356 Al-alloy is examined. The variability in ductility does not correlate to the global average microstructural parameters, such as dendrite cell size, Si particle size, and amount of porosity in the three-dimensional microstructure. Tensile fracture surfaces contain oxide films and residues of modifiers, fluxes, grain refiners, and mold release agents: EDS shows presence of elements such as O, Na, K, C, Ca, Fe, and S in these defects. The fracture path preferentially goes through the regions containing the defects. SEM quantitative fractography was used to estimate the total area fraction of such defects in the fracture surfaces of the tensile test specimens. The percent tensile ductility e shows strong quantitative correlation with the area fraction of the defects f in the corresponding fracture surfaces, which can be represented by the following simple equation. e = e 0 [ 1 − f ] n In this equation, e 0 and n are empirical constants. For the present data set, e 0 is equal to 15.84% and n is equal to 8.3. Thus, the variability in the ductility can be decreased through a reduction in the amount of processing defects via better process control.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have