Abstract

n-Butyllithium-initiated ring-opening polymerization of ethylene oxide with potassium t-butoxide in the mixture of benzene and dimethyl sulfoxide (DMSO) at 35 °C yielded corresponding “living” polymeric alkoxide. The molecular weight was well controlled on the basis of stoichiometric balance. Quantitative chain-end functionalizations, such as the amination, the azidation, and the thiolation of polymeric alkoxide, were performed. The yields were almost quantitative (over 98 mol%). The resulting products were characterized by the combination of 1H NMR spectroscopy, UV/Visible spectroscopy, FTIR, MALDI-TOF MS analysis, and size exclusion chromatographic analysis. Open image in new window

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.