Abstract

Slab quality affects the quality of hot rolled sheet significantly. There were serious transverse corner cracks on continuous casting slab of 510L steel plate in Panzhihua Steel before. Based on this, some effective countermeasures are put forward, such as the optimization of ratio of heat flux on narrow side and broad side of casting slab and mold powder, as well as the stabilization of casting speed and working condition of caster. With these countermeasures, transverse corner cracks on continuous casting slab have been significantly reduced, and the lines and peeling defects on hot rolled sheet reduce from 30% to 0.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.