Abstract

[Pb(Zr,Ti)(OAc)x(OR)y] acetate-alkoxide precursor was prepared by chelating from organic Pb, Zr and Ti alkoxides by their dissolution in various amounts of acetic acid (AcOH). The optimum mole ratio of (Pb+Zr+Ti) to AcOH for preparation gel is 1:7 and a pure perovskite phase is formed at 500 °C. At a low AcOH concentration, two-phase (pyrochlore and perovskite) regions are formed during gellation. During sintering, the decomposition of a pyrochlore phase and the formation of a perovskite phase takes place Dependences of dielectric permitivities and losses on temperature in final PZT ceramics were very similar and they were not influenced by the type of calcinate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.