Abstract

The rise in the use of polycarbonate (PC) calls for the development of after-use treatments. In this work, we describe a process for obtaining bisphenol A (BPA), phenol and isopropenyl phenol (IPP) from PC by hydrolysis at temperatures between 300 and 500 °C. The experiments were carried out in a steam atmosphere in the presence of MgO, CaO, Mg(OH) 2 or Ca(OH) 2 as catalysts, respectively. The results were compared with the hydrolysis of PC in the absence of any catalysts. All of these catalysts accelerated the hydrolysis of PC drastically, with MgO and Mg(OH) 2 being more effective than their Ca counterparts. The differences between oxides and hydroxides were negligible indicating the same mechanism for both, oxides and hydroxides. BPA was the main product at 300 °C, with a yield of 78% obtained in the presence of MgO. At 500 °C, BPA was mainly degraded to phenol and isopropenyl phenol (IPP). It can be shown that a combined process involving PC hydrolysis at 300 °C and BPA fission at 500 °C leads to high yields of phenol and IPP and the drastic decrease of residue.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.