Abstract

The products of pyrolysis, at 400°C in vacuo (1 Pa), of poly(ethyleneterephthalate) (PET) and poly(butyleneterephthalate) (PBT) were studied. The products were identified by gas chromatography/mass spectrometry technique. The highly volatile products of PET contained acetaldehyde, benzene, toluene, styrene and ethylbenzene and in the case of PBT, butadiene, tetrahydrofuran, vinylcyclohexene and ethylbenzene were the major products. A qualitative analysis of the products of low volatility revealed that the main components were benzoic acid, terephthalic acid, monovinyl esters of terephthalic acid and higher oligomers in the case of PET, whereas benzoic acid, monobutenyl esters of terephthalic acid and higher oligomers were the main products from PBT. The results obtained were in good agreement with those obtained from pyrolysis experiments, carried out directly in the mass spectrometer. Mechanisms to explain the occurrence of the different products are proposed.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call