Waste polypropylene (PP) has been pyrolysed to obtain mainly a liquid tar product of high yield (83.5%) with the balance as gas (15.5%) and a little residue (1.0%). The elemental composition of the PP tar was: C: 87.1%, H: 12.6% and O+others: 0.4% (by difference). The tar samples have been characterised by gas chromatography/mass spectrometry, heated-probe mass spectrometry and laser -desorption mass spectrometry (LD- MS), to give molecular mass distributions for comparison with molecular mass ranges indicated by size-exclusion chromatography (SEC). About 50% of the tar was soluble in 1-methyl-2-pyrrolidinone, the solvent used for SEC. It appeared to consist mostly of low molecular mass materials with elution time at 20-27 min. Mass ranges from SEC and LD-MS agreed approximately in showing the upper mass limit of the tar to be about 1200 u, consisting of aromatics, alkenes, dialkenes and only minor quantities of alkanes.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call