Abstract

Surface charge of pyroelectric nature is measured in poled hydroxyapatite ceramics. The average pyroelectric constant can range from 0.1 to 40 nC cm−2 K−1 at temperatures of 300–500 °C, while at 27–60 °C the value ranges from 15 to 64 nC cm−2 K−1. The higher temperature values are comparable to conventional pyroelectric ceramics such as LiTaO3 or PZT. The lower temperature values are four orders higher than those observed in bone and tendon.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.