Abstract

The pyroelectric properties of (Ba0.825+xCa0.175-x)(Ti1-xSnx)O3 ceramics with x = 0.0625, 0.0875 and 0.100 were investigated. Samples were fabricated using solid state reaction route and were exposed to IR lamp periodically to recorded open circuit voltage. Peak value of open circuit voltage was 0.8 V, 0.70 V and 0.53 V for x = 0.0625, 0.0875 and 0.1 samples, respectively. P–E loops were recorded for all the compositions under study. Further pyroelectric coefficient was estimated using P–E loops data. The values of pyroelectric coefficient estimated as 5.70 × 10−4C/m2 K, 5.5 × 10−4C/m2 K and 5 × 10−4C/m2 K for x = 0.0625,0.0875 and 0.1 samples.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.