Abstract

AbstractCooling crystallization was successfully carried out in a batch cooling crystallizer from impure acidic solutions to recover nickel as nickel sulfate salt with three different cooling rates. The compositions of the solutions included impurities of sodium, magnesium, chloride, and sulfuric acid to mimic industrial nickel electrowinning process solutions. The results show that NiSO4·6H2O mainly crystallized, and its solubility and purity decreased with the increase in the mass ratio of chloride to sulfate. Cooling rates did not have a significant influence on crystal purity; however, it did affect the filter cake moisture; lower moisture can be obtained with a lower cooling rate. The sequence of impurity removal efficiency from high to low was Cl > Na > Mg.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.