Abstract
Films of barium titanate were deposited by flash evaporation from tungsten and iridium crucibles in the presence of a low partial pressure of oxygen during the deposition. In a second more satisfactory method, a layer of TiO 2 was deposited by reactive cathodic sputtering followed by a layer of BaO deposited by evaporation from BaCO 3 in a platinum crucible. The thermal synthesis of BaTiO 3 was completed by heating the substrate of iridium or platinum at temperatures up to 1100°C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.