Abstract

A sulfonated poly(ether ether ketone) (SPEEK) membrane with fairly high degree of sulfonation (DS) swells excessively and even dissolves at high temperature. To solve these problems, sulfonated phenolphthalein poly(ether sulfone) (SPES-C, DS53.7%) is blended with the SPEEK matrix (DS55.1%, 61.7%) to prepare SPEEK/SPES-C blend membrane. The decrease in swelling degree and methanol permeability of the membrane is dose-dependent. Pure SPEEK (DS61.7%) membrane dissolves completely in water at 70°C, whereas the swelling degree of the SPEEK (DS61.7%)/SPES-C (40%, by mass) membrane is 29.7% at 80°C. From room temperature to 80°C, the methanol permeability of all SPEEK (DS55.1%)/SPES-C blend membranes is about one order of magnitude lower than that of Nafion® 115. At higher temperature, the addition of SPES-C polymer increases the dimensional stability and greater proton conductivity can be achieved. The SPEEK (DS=55.1%)/SPES-C (40%, by mass) membrane can withstand temperatures up to 150°C. The proton conductivity of SPEEK (DS55.1%)/SPES-C (30%, by mass) membrane approaches 0.16 S·cm −1, matching that of Nafion® 115 at 140°C and 100% RH, while pure SPEEK (DS55.1%) membrane dissolves at 90°C. The SPEEK/SPES-C blend membranes are promising for use in direct methanol fuel cells because of their good dimensional stability, high proton conductivity, and low methanol permeability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.