Abstract

In the paper the properties of concrete masonry unit (CMU) made from sedimentary lightweight aggregate (LWA) were investigated. The main variables include water to cementitious material ratio (W/CM), filling ratio of paste or mortar in voids between coarse aggregate particles (Fv), filling ratio of sand in mortar (Fm), and cement replacement level by slag (Sc). Test results of representative CMU specimens show that unit weight ranged from 1585 to 1743 kg/m3, which was 30-25% lower than that for a normal weight CMU (2300 kg/m3); compressive strengths ranged from 8.4 to 18.7 MPa; water absorption was found to vary between 0.05 to 0.13 g/cm3; and thermal conductivity ranged from 0.27 to 0.41 W/mK. The research findings demonstrate that the use of sedimentary LWA as coarse aggregate in various concrete mixtures could produce high performance lightweight CMU, which comply with the requirements of Chinese National Standards (CNS) standards.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.