Abstract
The effects of a recently developed shrinkage-reducing admixture on high-performance concrete properties are described. High-performance concrete mixtures containing silica fume were cast with and without shrinkage-reducing admixture. The mechanical properties, drying shrinkage, and resistance to restrained shrinkage cracking were investigated. The results show that the shrinkage-reducing admixture effectively reduced the shrinkage of high-performance concrete, and resulted in a significant decrease in restrained shrinkage cracking.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.