Abstract

Polyurethanes were synthesized using the high functional 4,4′-diphenylmethane diisocyanate (MDI), polyester polyol, and 1,4-butane diol. The synthesized polyurethanes were analyzed using differential scanning calorimeter (DSC), dynamic mechanical thermal analysis (DMTA), Fourier transform infrared (FTIR) spectrometer, and swelling measurement using N,N′-dimethylformamide. From the result of thermal analysis by DSC and DMTA, single Tgs were observed in the polyurethane samples at all the formulated compositions. From this result, it is suggested that the polyurethanes synthesized in this study have crosslinked structure rather than the phase-separated segmented structure because of the high functionality (f = 2.9) of the MDI. By annealing the polyurethane samples using DSC, the Tgs were increased by 4.7∼16.0°C at the various annealing temperatures. From the results of FTIR and swelling measurement of polyurethanes, it is suggested that the increase of Tg of the polyurethanes by annealing is not due to increase of the hydrogen bond strength but mainly due to the increase of the crosslink density. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 78: 624–630, 2000

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.