The dielectric properties of Ba(Mg1/3Ta2/3)O3 (BMT) microwave thin films synthesized by an in situ pulsed-laser deposition (PLD) process were compared with those prepared by a two-step PLD process. The onset of crystallization for the BMT films is approximately 400°C, when in situ deposited, and is approximately 550°C, when two-step processed. Dielectric measurements indicate that complete crystallization for BMT films can be achieved only by processing the films at a sufficiently high temperature, which is 600°C for an in situ PLD process and is 800°C for a two-step PLD process. The microwave dielectric properties of BMT films, which were directly measured by an evanescent microwave probe (EMP) technique at 2.65 GHz measuring frequency, increase with substrate temperature, resulting in dielectric constant K=33.3 and dissipation factor tan δ =0.0158.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.