Abstract
The promoting effect of secondary phase particles on the refinement of matrix grains in a series of Mg–Y1.5–Nd0.6-Zn.x (x=0, 0.2, 0.4, 0.8, 1.3) alloys deformed by friction stir processing (FSP) was investigated in this study. The volume fraction of secondary phase in the alloys increased with increment of Zn, and most of the secondary phases were broken into nano-sized particles and dispersed in the matrix during thermal mechanical processing. The resulting fine particles had a remarkable promoting effect on the grain refinement of the Mg matrix during mechanical processing, thermal deformation, and cooling with increasing volume fraction of the secondary phase. For example, the grains of Mg–Y1.5–Nd0.6–Zn1.3 alloy were refined to an average size of 28nm, compared with the more than 100nm grain size of the Mg–Y1.5–Nd0.6 alloy.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.