Abstract

The profluorescent nitroxide, 1,1,3,3-tetramethyldibenzo[ e, g]isoindolin-2-yloxyl (TMDBIO) was investigated as a probe for the radical-mediated degradation of stabilised polypropylene. TMDBIO has been previously shown to be a sensitive probe for free-radical degradation during the thermo-oxidation of unstabilised polypropylene. Here we report on the effect that adding hindered phenol or phosphite stabilisers to polypropylene has on the free-radical sensing ability of TMDBIO during thermo-oxidation. In addition, novel dual-functional, hindered phenol containing profluorescent nitroxides, 5-[2-(4-hydroxy-3,5-di- tert-butylphenyl)ethenyl]-1,1,3,3-tetramethylisoindolin-2-yloxyl (HSTMIO) and its derivatives were investigated as probes for the radical-mediated degradation of polypropylene. These dual-functional probes were shown to be efficient stabilisers for polypropylene during thermo-oxidation at 150 °C in oxygen and sensors of thermo-oxidation during its early stages, in the so-called “induction period”.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.