Abstract: Pyrolysis of washed poly (ethylene terephthalate) (PET) plastic wastes was performed, pyrolysis products yields were determined and epoxy composite was prepared with char additive in this study. The pyrolysis runs were carried out in the temperature range of 300-700°C in order to indicate the effects of pyrolysis temperature on products. The char from pyrolysis was used in the production of epoxy composite material and char replaced at 10 to 50 wt% of the epoxy resin. Mechanical properties, namely tensile strength, surface hardness and electrical properties were determined for the epoxy composite materials. The tensile strength increased 131% at the dose of 50% for char obtained at 300°C. The hardness was improved up to 83-89 shore D from 80 shore D by the PET char additive in the composite. Epoxy composite material obtained by PET pyrolysis char additive obtained at 300°C showed the better behavior in terms of elongation at break and tensile strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.