Abstract

Technology for obtaining peat and peat-wood composite materials by the explosive autohydrolysis method without using synthetic binders was developed. The optimal conditions of an explosive autohydrolysis of peat and peat in the presence of wood were found: pressure 1.62 MPa, temperature 210°C, treatment duration of 10 min in an explosive autohydrolysis reactor. Peat and peat-wood composite materials were obtained. In their strength characteristics (bending strength up to 14.68 MPa) and heat conductivity these materials compare well with the conventional heat-insulating materials and can be used as construction materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.