Abstract

Dry reforming of glycerol has been carried out over alumina-supported Ni catalyst promoted with lanthanum. The catalysts were characterized using EDX, liquid N2 adsorption, XRD technique as well as temperature-programmed reduction. Significantly, catalytic glycerol dry reforming under atmospheric pressure and at reaction temperature of 1023 K employing 3 wt%La–Ni/Al2O3 catalyst yielded H2, CO and CH4 as main gaseous products with H2:CO < 2.0. Post-reaction, XRD analysis of used catalysts showed carbon deposition during glycerol dry reforming. Consequently, BET surface area measurement for used catalysts yielded 10–21% area reduction. Temperature-programmed gasification studies with O2 as a gasification agent has revealed that La promotion managed to reduce carbon laydown (up to 20% improvement). In comparison, the unpromoted Ni/Al2O3 catalyst exhibited the highest carbon deposition (circa 33.0 wt%).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.