Abstract

Modification of tars with formalin (37 % aqueous solution of formaldehyde) was carried out using various acids as process catalysts with the aim of obtaining new binding materials for road construction. H2SO4, HCl, H3PO4, and СH3COOH were used as catalysts. The modification process was carried out in the temperature range of 378-403 K and for a duration of 0.6-1.0 h. The rheological properties of tars modified with formaldehyde at 333, 343, and 353 K were studied and a comparison of the rheological properties of the obtained bituminous binder materials with oxidized bitumens was carried out.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.