The process for producing the electrode material LiCoPO4 modified by the lithium-conducting solid electrolyte Li1.3Al0.3Ti1.7(PO4)3 (LATP) was studied. To create a composite consisting of an electrochemically active substance and an electrically conductive additive distributed uniformly between LiCoPO4 particles, a peroxide solution of a LATP precursor was used. After annealing at 700°C, the two-phase composite LiCoPO4/LATP was obtained, the conductivity of which was two orders of magnitude higher than that of binary lithium cobalt phosphate at room temperature.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.