Abstract
In this study, it was aimed to produce Al-matrix composite materials with B4C-SiC and B4C-Y2O3 particle reinforcement using the Powder Metallurgy (PM) method. In the composites in which the reinforcement materials were used at different particle sizes and ratios, AA2024 powders were selected as the matrix material. The powders were homogeneously mixed and compacted at room temperature under a pressure of 525 MPa. The raw specimens were sintered by keeping them at different temperatures for 45 minutes. The composite materials were subjected to wear tests, and their hardness and density values were investigated. In the study, the effects of reinforcement materials added to the matrix at different particle sizes and ratios on wear resistance, hardness, and density at different temperatures were examined.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.