Abstract

Although 6.5wt% high silicon electrical steel has pretty excellent soft magnetic properties, it is hard to be obtained by cold rolling at room temperature, by virtue of appearance of ordered phases in this alloy. In this research we report that very thin 6.5wt%Si composite sheet with 0.05-0.08mm thickness was fabricated by proper heat treatment and cold rolling after hot deformation. The 6.5wt%Si composite plate exhibits some extent of ductility at room temperature when the stage of hot deformation was finished. The effect of heat treatment on mechanical properties of this composite plate was investigated by optical microscope. After heat treatment, ductility of this composite plate is increased due to the ordered DO3phase transformation inhibited by cooling fast. It is provided a referable method to produce 6.5wt% high silicon steel with conventional forming process.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.