Abstract

A technology has been developed for obtaining fuel tablets with the compositions (U, Th)O2, (U, Th, Ca)O2, and (U, Th)O2+MgO by combined precipitation of uranium, thorium, magnesium, or calcium components from inert solutions, followed by heat treatment of the powders, compression into pellets, and sintering of the pellets. Work on optimizing the technological processes for obtaining fuel pellets so as to obtain good pellet quality was performed. The effect of the properties of the precipitates and powders, fabricated using different technological regimes on the properties of the finished objects was studied. The work includes detailed investigations of powders (x-ray phase analysis, electron-microscopic investigation) and sintered fuel tablets (change in the geometric dimensions as a result of sintering, determination of the density, and study of the microstructure). The behavior of fuel compositions (U, Th)O2 and (U, Th)O2+MgO in contact, with coolants under conditions where the fuel elements become unsealed was studied: with water at 300°C and sodium at 700°C. 3 figures, 3 tables, 6 references.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.