Abstract

The paper provides a flow sheet of the phosphorus slag processing to produce precipitated silica (white soot). The process conditions for opening phosphorus slag at the I stage of leaching have been selected: the nitric acid concentration is 3.5 mol/dm3; the ratio S:L = 1:3.5; the temperature is 60 oС; and the process duration is 1 hour. The parameters of the white soot production II stage have been determined: the HNO3 concentration is 6.5 mol/dm3; the ratio S:L = 1:3.5; the temperature is 50 oС; and the process duration is 1 hour. The temperature effect on the white soot structure and the specific surface have been established. At optimal process parameters, the white soot batches have been obtained with the main SiO2 component content of 88.2 and 90.5 %, and a specific surface of 170 and 182 m2/g, respectively. The through recovery of silicon into a commercial product is 98.0 % of its initial content in slag.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.