Abstract
Coatings with the 0.7BaTiO3–0.3BiScO3 solid-solution composition were formed on palladium and single-crystal (001) SrTiO3 substrates using a polymeric metal citrate precursor. Solutions of TiOCl2, Ba(NO3)2, Sc(NO3)3, and Bi(NO3)3 were mixed with citric acid and polymerized with ethylene glycol. Stable mixed-metal citrate solutions were formed at pH > 9 and used for coatings. The phase and composition of powders and coatings were characterized using DTA, TGA, SEM, TEM, and X-ray diffraction. Single-phase cubic 0.7BaTiO3–0.3BiScO3 solid solutions formed at 600°C. Coatings on Pd using precursors doped with 5 wt% lithium nitrate were dense after sintering at 950°C/1 h. Coatings without lithium nitrate required 1050°C/50 h to densify. Coatings on SrTiO3 heat-treated at 1150°C were dense but formed a (Sc,Ti)-rich second phase.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Applied Ceramic Technology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.