Abstract
The deep drawing of SiC/2024Al composites using pulse current heating were designed and established in this works. The whole process system mainly include pulse current heating system, electrode lifting system, temperature control system and deep drawing forming system. In addition, the feasibility of thermal deep drawing using pulse current heating was experimentally investigated and the optimal process parameters were explored to ensure defect-free products. The temperature of specimen is up to around 673K at a rate of 13.5K/s under the current density of 21.7A/mm2. The stainless steel inserts make temperature difference reducing by 73.3%. Moreover, the workpiece was successfully deep drawn and exhibited good surface quality. The dimensional accuracy achieved within ±0.2mm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.