Abstract

Abstract There is a problem in obtaining a suitable impact strength of the padding weld after cladding with a martensitic filler metal. Too low annealing temperature below 580°C and the excessive annealing temperature above 650°C do not provide adequate impact strength of the padding weld. A heat treatment technology for mixed joints has been developed based on the results of the microscopic observations, X-ray diffraction measurements and transmission electron microscope examination. The problem was identified and a special technology of heat treatment for the dissimilar joint was elaborated. This technology provides a high impact resistance of the padding weld and an appropriate properties of the base material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.