Abstract
The spatially resolved identification of active sites on the heterogeneous catalyst surface is an essential step toward directly visualizing a catalytic reaction with atomic scale. To date, ferrous centers on platinum group metals have shown promising potential for low-temperature CO catalytic oxidation, but the temporal and spatial distribution of active sites during the reaction and how molecular-scale structures develop at the interface are not fully understood. Here, we studied the catalytic CO oxidation and the effect of co-adsorbed hydrogen on the FeO2-x/Ir(111) surface. Combining scanning tunneling microscopy (STM), isotope-labeled pulse reaction measurements, and DFT calculations, we identified both FeO2/Ir and FeO2/FeO sites as active sites with different reactivity. The trilayer O-Fe-O structure with its Moiré pattern can be fully recovered after O2 exposure, where molecular O2 dissociates at the FeO/Ir interface. Additionally, as a competitor, dissociated hydrogen migrates onto the oxide film with the formation of surface hydroxyl and water clusters down to 150 K.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.