Abstract

In this study, an alkaline-catalyzed sulfolane/water solvent system was developed for isolating high-purity and antioxidative lignin from willow (Salix matsudana cv. Zhuliu). Optimization of the pretreatment conditions such as temperature, sulfolane/water ratio, and alkaline catalyst (NaOH) dosage were comprehensively investigated for effective lignin extraction from willow. The 44.4% of lignin was recovered from the biomass with 54% of delignification in 50/50 (w/w) sulfolane/water system at 170 °C. As the addition of the alkaline catalyst (NaOH) increased to 4%, the delignification yield was increased up to 94% with about 70% of lignin recovery yield. The recovered lignin was comparatively investigated with its control, milled wood lignin (MWL). The β-O-4 linkages and phenolic hydroxyl were well preserved in the extracted lignin fractions with the sulfolane/water system. Furthermore, excellent radical scavenging ability was observed with the extracted lignins by sulfolane/water pretreatments owing to rich phenolic hydroxyl groups in the lignins. Hence, systematical investigation on the lignin properties and potential applications under sulfolane organosolv pretreatment would promote the utilization of lignin in biorefinery processes.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.