Abstract

Densification of boron carbide (B4C) was studied by pressureless sintering at temperatures ranging from 2108° to 2226°C with Al gas and Si compound gas derived from SiC. High purity boron carbide compacts attained a bulk density of a nearly full density (2.455 g/cm3) after being sintered at 2226°C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.