Abstract

A neglected mechanism for pressure-responsive color change is demonstrated using cellulose acetate composites prepared by direct (solvent) immersion annealing (DIA), with different loadings of activated charcoal filler. Namely, compressive plastic deformation of the translucent cellulose acetate leads to a decrease in the optical path length and a concomitant increase in the visibility of the opaque contrasting filler. Composites bearing 1-7 wt% activated charcoal exhibited a linear relationship between applied pressure and resulting pressure mark brightness in the range of 12-56 MPa. Comparison of pressure mark patterns with cross-sectional scanning electron microscopy (SEM) supports the importance of the porous morphology arising from DIA for the tuning of the pressure indicator sensitivity. A simple ball drop test is used to illustrate the robustness and utility of these indicators in optical impact assessment.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call