Abstract

Many studies on superconductivity of boron-doped diamond (BDD) have been done, and it is well known that the superconducting transition temperature Tc of BDD films depend on the boron concentration and the growth direction. Uniaxial like pressure along (111) direction was applied on boron-doped (111) diamond films synthesized by CVD method using a diamond-anvil cell (DAC) up to 18.5 GPa. The Tc was decreased as previous report, however the changing rate is smaller than other experiments with hydrostatic pressures and a theoretical prediction.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.