A method for the preparation of zirconia-toughened mullite using dc plasma is presented. An indigenously developed 50-kW thermal plasma reactor is used for the preparation of zirconia-toughened mullite using a dissociated zircon and alumina mixture. Both XRD and SEM studies of the product confirmed the formation of mullite and zirconia. The zirconia grew as equiaxed grains of uniform size (~5 μm) in a mullite matrix.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.