Abstract

Abstract - The dissolution of glass in highly alkaline reaction mixtures and the impact of this phenomenon on zeolite coating formation were investigated. Coating samples were prepared and characterized by X-ray diffraction (XRD), field emission gun scanning electron microscopy (FEGSEM) and thermogravimetry (TG). It was demonstrated that zeolite X coatings might be prepared on soda-lime glass. Glass dissolved to some degree, up to 2% of its original mass, in the reaction mixtures for the conditions investigated. This dissolution affected the zeolite synthesis taking place on the glass surface, resulting in phases different from those obtained on inert metal surfaces in some cases, especially for the use of reaction mixtures with relatively high Si/Al ratios. The percentage of dissolution of glass plates increased with their decreasing thickness, indicating a surface phenomenon for the dissolution. The stabilities of the coatings, which varied with the synthesis conditions, benefited from the addition of extra thin layers of polyacrylic acid.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.