Abstract

With the rapid development of the electric power industry in China, the amount of fly ash discharged is growing day by day, which brings great harm to the production industry and people’s living conditions. In this article, hydro-thermal method and alkali fusion -hydro-thermal method have been used to prepare 4A zeolite from coal fly ash. The results indicate that the optimum conditions (calcination temperature 850°C, ratio of silicon to aluminum in raw material 0.8, alkalinity of NaOH 2.5mol/L, the aging time 6h, crystal temperature 90°C and crystal time 24h), the specific surface area of the prepared zeolite is 605.6m2/g. The synthesized 4A zeolite has a uniform particle size with a narrow distribution. Its shape is cube and in rules, and all its properties are close to 4A zeolite purchased in the market.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.