Abstract

High quality bulk YBa2Cu3O7−x was synthesized by fusing stoichiometric amounts of yttrium and copper nitrates and barium hydroxide in air, using an ordinary Bunsen burner. The starting materials go through a short-lived liquid phase yielding a solid black product which was subsequently heat treated (900 °C, 18–24 h in air, followed by 500 °C, 5 h in O2). These materials were greater than 99% phase pure with CuO as the only other phase and they exhibited a transition temperature of 92 K, a 15.5% perfect diamagnet response (field cooled). This synthesis represents an improvement over the much more labor and time intensive conventional methods in that it allows high quality materials of various compositions to be prepared quickly.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.