Abstract

Pyrochlore-structured materials are very important materials due to their structural and conducting properties. These properties can be further modified by changing processing conditions. In the present study, pyrochlore (Y2Ti2O7) is synthesized using high-energy ball milling. During various stages of ball milling, the ball-milled powder is taken for investigating the structural and thermal properties. The replacement of Ti2O3 by TiO2 in nominal composition leads to lower ball milling duration to form Y2Ti2O7. Differential thermal analysis showed the single exothermic peak below 800 °C, which indicates formation of disordered pyrochlore phase. The as prepared powders (40-h ball milled) were compacted and heat treated at 1,450 °C for 12 h. The conductivity of sintered sample is found to be one order higher than earlier reported pure Y2Ti2O7 pyrochlore.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.