Abstract

In this paper, Y2O3-Al2O3-ZrO2 nano-ceramic coatings were prepared on 316L stainless steel substrate at 600°C for 0.5 hour by sol-gel method, using Y(NO3)3•6H2O, ZrO(NO3)•2H2O and Al(NO3)3•9H2O as raw materials, hexamethylenetetramine as catalyst. Phases and morphology of these coatings were characterized by XRD, SEM and EDS. Effect of heat treatment temperature on microstructure of the coatings was studied. Y2O3-Al2O3-ZrO2 coatings with grain size about 50nm tightly integrated with metal substrate after densely sintering at 600°C. The grain sizes have grown up with increasing temperature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.