Abstract

Ultra‐fine composite fibers made from poly(vinyl alcohol) (PVA)/silatrane, an inexpensive and moisture‐stable silicon‐containing compound, were prepared by a combined sol–gel processing and electrospinning technique with average diameters ranging between 119 and 405 nm. These fibers were subsequently converted to ultrafine silica fibers by calcination treatment, with the aim of producing a silica structure with a high surface area‐to‐mass ratio. Upon calcination at 500°C, the PVA/silica composite fibers were converted into amorphous silica fibers, while calcination of the composite fibers at temperatures ≥700°C resulted in the formation of cristobalite fibers. The average diameter of these silica fibers ranged between 162 and 213 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.