Abstract

AbstractA combined process of carbothermal reduction in vacuum and acid leaching is proposed to produce TiC from titanium bearing blast furnace (BF) slag from Pan Steel in Panzhihua city in China. Thermodynamics calculation shows that TiC can be obtained in the appropriate temperature and pressure range. Moreover, the results of the experiment indicate that TiC can be prepared by the combined process. The optimized parameters include particle size of original slag ideally below 200 mesh, reduction temperature of 1400°C, pressure of 1~10 Pa and mass ratio of slag and reduction (carbon powder) of 100/38. The x value in TiC

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.