This paper describes the reduction of titanium dioxide with a mixture of silicon carbide and silicon powders at a temperature of 1550°C under vacuum. It has been shown that the use of the combined reductant enables the preparation of the ternary phase Ti3SiC2 through concurrent carboand silicothermic processes. The optimal compositions for Ti3SiC2 formation are TiO2 + (1.5–x)SiC + 2xSi with x = 0.4–0.5. The Ti3SiC2 yield then reaches 96 wt %.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.