This paper using high energy ball milling (HEM), researched has discussed the preparation of Al-CNT compound materials at the different milling times, rotary speeds, amount of CNT and sinter technology for their properties of hardness and density and for the preparation the Al-CNT. The milling time is about 30 to 100 min, with a rotational speed of about 300-600/rpm and the wt% of CNT being 0-5%. This paper has analyzed the XRD patterns. SEM and STM micrograph, and the results showed that the Al material could be reinforced by CNT using HEM. The hardness of Al-CNT is 75 HB with a density of 2.65 g/cm3 when milling is carried out for 90 min, at CNT being 3%. Keywords: High energy milling(HEM), Al-CNT, compound material, rotary speeds, Carbon Nanotubes

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.