This study focuses on the synthesis of SrVO3 through the reduction of Sr2V2O7 by annealing in a reducing atmosphere. The effects of annealing temperature and annealing duration on Sr2V2O7 were investigated. The X-ray powder diffraction pattern showed that stoichiometric changes to Sr2V2O7 were achieved only at an elevated annealing temperature of 1000 °C in a reducing atmosphere, and that the desired SrVO3 was obtained only after 144 h of annealing. Further investigation of SrVO3 was performed using X-ray photoelectron spectroscopy, which confirmed that the reduction of V5+ found in Sr2V2O7 to V4+ found in SrVO3 was achieved.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.