Abstract

The silicon carbide (SiC) powder is covered with polycarbosilane (PCS), N-Methyl pyrrolidone (NMP) is a solvent, polyethersulfone (PES) is a bonding aid, using phase-phase and solid-phase sintering process combined with a step-by-step molding to prepare a symmetrical structure of silicon carbide hollow fibers, and determine the membrane’s perforation and purification and purity of the water distribution and the circumference of the membrane. The results show that the SiC membrane tube is a finger-hole structure layer-spongy structure layer-finger-hole structure structure, the optimal sintering temperature is at 1200 °C, the size of the prepared ceramic membrane aperture is concentrated in about 0.9 μm, and the pure water flux is 2.832m3 / (m2⋅h).